High strength-to-weight ratio and outstanding corrosion resistance are properties inherent to titanium alloys. These properties have led to a wide range of successful applications that almost always require high reliability for markets such as power generation, aerospace, sporting equipment, automotive, chemical processing and medical.
Ti-6Al-4V is the most widely used titanium alloy composition. It features good machinability and excellent mechanical properties. MetcoAdd Ti-6Al-4V ELI are atomized spheroidal titanium powders for additive manufacturing applications. Components manufactured from MetcoAdd Ti-6Al-4V ELI powders offer the best all-around performance for a variety of applications where weight reduction and/or corrosion resistance is a concern for industries that include aerospace, automotive and marine structures. The composition of MetcoAdd Ti-6Al-4V ELI also has numerous applications in the medical industry.
MetcoAdd Ti-6Al-4V ELI powders meet the chemical composition of ASTM B348-13 Grade 23 and Grade 5. The lower oxygen content of Grade 23 allows users either more flexibility during manufacturing and subsequent heat treatment or to take advantage of the higher ductility and fracture toughness of low oxygen titanium.
The processes used to manufacture MetcoAdd Ti-6Al-4V ELI are tightly controlled to ensure repeatable and consistent powder quality that results in consistent printing perform.
Key Selection Criteria:
Density
ρ2.3 g/cm³ at 20 °C
apparent density, min
Particle size D10
D1016 - 30 μm
MetcoAdd Ti-6Al-4V ELI-A
Particle size D50
D5030 - 40 μm
MetcoAdd Ti-6Al-4V ELI-A
Particle size D90
D9040 - 50 μm
MetcoAdd Ti-6Al-4V ELI-A
Particle size range
drange15 - 45 µm
MetcoAdd Ti-6Al-4V ELI-A: -45 +15µm; MetcoAdd Ti-6Al-4V ELI-B -105 +45µm
Melting point
Tm1635 °C
Hall flow
HF40 s/50g at 20 °C
max MetcoAdd Ti-6Al-4V ELI-A
Application areas
Additive manufactured components using Laser Powder Bed Fusion (L-PBF) or Electron Beam Melting (EBM) for: Aerospace and defense; Automotive and racing; Maritime applications; High-end sports equipment; Medical and dental; Jewelry and art
Availability
Stock
Chemical composition
Ti-6Al-4V Extra Low Interstitials (ELI)
Distribution
Global
Export control
MetcoAdd Ti-6Al-4V ELI powder and printed products are subject to the U.S. Export Administration Regulation (EAR). These products are classified as ECCN 1C002.b.3 with NS Column 2, NP Column 1, AT Column 1 controls within the regulation. All shipments of MetcoAdd Ti-6Al-4V ELI powder and printed products outside of the United States, in any quantity, may require an export license through BIS (Bureau of Industry and Security, U.S. Department of Commerce). Complete information regarding licensing requirements and policies, as well as the full EAR text, can be found at www.bis.doc.gov.
Handling recommendations
Keep in the original container, or an approved alternative, tightly closed when not in use; Store and handle away from heat, sparks, open flame or any other ignition source; Use explosion-proof electrical (ventilating, lighting and material handling) equipment; Store in a segregated and approved area that is dry, cool and well-ventilated, away from incompatible materials, food and drink; Protect contents from direct sunlight
Morphology
Spheroidal
Order number
MetcoAdd Ti-6Al-4V ELI-A: 1099837, MetcoAdd Ti-6Al-4V ELI-B: 1099838
Packaging size
2.5 kg (approx. 5.5 lbs)
Processing history
Atomization
Processing methods
Laser Powder Bed Fusion (L-PBF), Electron Beam Melting (EBM)
This material data has been provided by Oerlikon Metco.