Designed for Processing in Laser Powder Bed Fusion (PBF-LB) Systems


MetcoAdd™ H230-A is a nickel-based powder product with chemistry similar to AMS 5891 bar material. 


Room temperature static properties of PBF-LB processed and heat treated material coupons have been shown to be comparable to those of AMS 5891. Elevated temperature tensile and creep rupture data may be made available upon request. 


For reference purposes Oerlikon has processed MetcoAdd H230-A using 40 μm layer thickness to provide data below. Properties may be optimized based on application specific requirements.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

4.5 - 5 g/cm³

Show Supplier Material materials with Bulk density of 4.5 - 5 g/cm³

typical apparent density

Particle size D10

25 μm

Show Supplier Material materials with Particle size D10 of 25 μm

nominal values by laser diffraction

Particle size D50

35 μm

Show Supplier Material materials with Particle size D50 of 35 μm

nominal values by laser diffraction

Particle size D90

49 μm

Show Supplier Material materials with Particle size D90 of 49 μm

nominal values by laser diffraction

Particle size range

15 - 45 µm

Show Supplier Material materials with Particle size range of 15 - 45 µm

ASTM C 1070 (Microtrac)

Thermal

PropertyValueComment

Melting point

1327 - 1455 °C

Show Supplier Material materials with Melting point of 1327 - 1455 °C

± 10 °C

Rheological Properties

PropertyTemperatureValueComment

Hall flow

23.0 °C

20 s/50g

Show Supplier Material materials with Hall flow of 20 s/50g

ASTM B213, max (typical)

Technological properties

Property
Application areas

Aerospace: Engine components, Power Generation: Gas turbine components, Industrial: Components requiring high temperature corrosion resistance for chemical, metallurgical and mineral process industries

Availability

Stock

Chemical composition

NiCrWMoAlTi

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Morphology

Spheroidal

Order number

1300725

Packaging size

4.5 kg/ 10 lb approx.

Processing history

Gas atomized (Argon)

Processing methods

Laser Powder Bed Fusion (PBF-LB)