H13 Hot Work Tool Steel for Laser Powder Bed Fusion (PBF-LB) or Directed Energy Deposition (DED) Systems

Want to keep this datasheet? Save it now in your required format

Description

Designed for Processing in Laser Powder Bed Fusion (PBF-LB) or Directed Energy Deposition (DED) Systems


MetcoAdd™ H13-A and H13-B are martensitic, iron-chromium, air-hardenable steel powders powder products with chemistries similar to AISI H13, ASTM H13, SAE H-13 and Werkstoff No. 1.2344 / X40CrMoV 5-1-1. 


Room temperature static properties of PBF-LB processed and heat treated material coupons have been shown to be comparable to those of AMS 6408. 


For reference purposes Oerlikon has processed MetcoAdd H13-A using fixed parameters and 40 μm layer thickness to provide data below. Additional testing has been performed by an extensive network of consortia and customer partners on a broader range of machine types. Properties may be optimized based on application specific requirements.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

4 g/cm³

Show Supplier Material materials with Bulk density of 4 g/cm³

typical apparent density, min

Particle size D10

21 μm

Show Supplier Material materials with Particle size D10 of 21 μm

nominal values by laser diffraction; H13-A

Particle size D50

34 μm

Show Supplier Material materials with Particle size D50 of 34 μm

nominal values by laser diffraction; H13-A

Particle size D90

50 μm

Show Supplier Material materials with Particle size D90 of 50 μm

nominal values by laser diffraction; H13-A

Particle size range

15 - 45 µm

Show Supplier Material materials with Particle size range of 15 - 45 µm

ASTM C 1070 (Microtrac); MetcoAdd H13-A: -45 +15µm; MetcoAdd H13-B: -90 +45µm

Thermal

PropertyValue

Melting point

1371 - 1482 °C

Show Supplier Material materials with Melting point of 1371 - 1482 °C

Rheological Properties

PropertyTemperatureValueComment

Hall flow

23.0 °C

25 s/50g

Show Supplier Material materials with Hall flow of 25 s/50g

ASTM B213, max H13-A

Technological properties

Property
Application areas

Hot work dies for casting, Casting dies for aluminum and magnesium, Hot forging and stamping dies, Hot shear blades, Plastic injection molds

Availability

Stock

Chemical composition

Fe 5Cr 1Mo 1Si 1V 0.4C

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Morphology

Spheroidal

Order number

H13-A: 1100784, H13-B: 1100785

Packaging size

4.5kg / 10 lb approx.

Processing history

Gas atomized (Argon)

Processing methods

H13-A: Laser Powder Bed Fusion (PBF-LB), H13-B: Directed Energy Deposition (DED)