Nickel Alloy X for Laser Powder Bed Fusion (PBF-LB)

Want to keep this datasheet? Save it now in your required format

Description

Optimized for Processing in Laser Powder Bed Fusion (PBF-LB)


MetcoAdd™ HX-D is a nickel-based solid solution strengthened powder product with chemistry similar to AMS 5536, EN 2.4665 and UNS N06002. This material has been optimized to mitigate cracking when processing with laser powder bed fusion. 


Room temperature static properties of PBF-LB processed and heat treated material coupons have been shown to be comparable to those of AMS 5536 plate and well in excess of AMS 5390 cast material. Elevated temperature tensile and creep rupture data may be made available upon request. 


For reference purposes Oerlikon has processed MetcoAdd HX-D using 40 μm layer thickness to provide data below. Properties may be optimized based on application specific requirements.

Properties

General

Density

ρ

4 g/cm³ at 20 °C

typical apparent density, min

Particle size D10

D10

18 μm

nominal values by laser diffraction

Particle size D50

D50

28 μm

nominal values by laser diffraction

Particle size D90

D90

42 μm

nominal values by laser diffraction

Particle size range

drange

15 - 45 µm

ASTM C 1070 (Microtrac)

Thermal

Melting point

Tm

1374 - 1397 °C

± 10 °C

Rheological Properties

Hall flow

HF

20 s/50g at 20 °C

ASTM B213, max

Technological properties

Application areas

Aerospace: Gas turbine and airframe parts; Power Generation: Gas turbine parts; Parts for petrochemical applications; Industrial furnace components; Structural components

Availability

Stock

Chemical composition

NiCrFeMo

Distribution

Global

Handling recommendations

Blend contents prior to use to prevent segregation; Keep in the original container, or an approved alternative, tightly closed when not in use; Powder from previously opened containers should be stored in a humidity-controlled environment

Morphology

Spheroidal

Order number

1301896

Packaging size

4.5kg / 10 lb approx.

Processing history

Gas atomized (Argon)

Processing methods

Laser Powder Bed Fusion (PBF-LB)

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.