UNI 6904 Grade X16CrNi2314

.XLSX
.PDF
Save

Chemical properties

Element

Weight %

Comment

Fe

57.72 - 66 %

Cr

22 - 24 %

Ni

12 - 15 %

S

0 - 0.03 %

Si

0 - 1 %

More

This material data has been provided by MetalInfo.