Description

Primary standard name

Chemical properties

Element

Weight %

Comment

Fe

98.13 - 99.03 %

C

0.42 - 0.5 %

Mn

0.4 - 0.9 %

Si

0.15 - 0.4 %

P

0 - 0.04 %

More

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.