SAE J407 Grade 94B15H

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyValueComment

Elastic modulus

190.0 - 210.0 GPa

Show Material materials with Elastic modulus of 190.0 - 210.0 GPa

Typical for Steel

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Chemical properties

PropertyValueRelated Standards

Boron

0.0005 %

Show Material materials with Boron of 0.0005 %

SAE J407

Carbon

0.12 - 0.18 %

Show Material materials with Carbon of 0.12 - 0.18 %

SAE J407

Chromium

0.25 - 0.55 %

Show Material materials with Chromium of 0.25 - 0.55 %

SAE J407

Copper

0.35

Show Material materials with Copper of 0.35

SAE J407

Iron

99.9949 - 99.9989 %

Show Material materials with Iron of 99.9949 - 99.9989 %

SAE J407

Manganese

0.7 - 1.05 %

Show Material materials with Manganese of 0.7 - 1.05 %

SAE J407

Molybdenum

0.08 - 0.15 %

Show Material materials with Molybdenum of 0.08 - 0.15 %

SAE J407

Nickel

0.25 - 0.65 %

Show Material materials with Nickel of 0.25 - 0.65 %

SAE J407

Phosphorus

0.035

Show Material materials with Phosphorus of 0.035

SAE J407

Silicon

0.15 - 0.35 %

Show Material materials with Silicon of 0.15 - 0.35 %

SAE J407

Sulfur

0.035 - 0.05 %

Show Material materials with Sulfur of 0.035 - 0.05 %

SAE J407