General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 9 g/cm³ Show Material materials with Density of 9 g/cm³ | Typical for Cobalt Superalloy |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 6E-7 - 8.7E-6 1/K Show Material materials with Coefficient of thermal expansion of 6E-7 - 8.7E-6 1/K | Typical for Cobalt Superalloy |
Chemical properties
Property | Value |
---|---|
Carbon | 1.1 - 1.7 % Show Material materials with Carbon of 1.1 - 1.7 % |
Chromium | 26 - 33 % Show Material materials with Chromium of 26 - 33 % |
Iron | 3 % Show Material materials with Iron of 3 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 1 % Show Material materials with Molybdenum of 1 % |
Nickel | 3 % Show Material materials with Nickel of 3 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.4 - 2 % Show Material materials with Silicon of 0.4 - 2 % |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % |
Tungsten | 7 - 9.5 % Show Material materials with Tungsten of 7 - 9.5 % |