SAE J775 Grade XEV-B

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Carbon

0.5 %

Show Material materials with Carbon of 0.5 %

Chromium

20.5 %

Show Material materials with Chromium of 20.5 %

Iron

62.65 - 100 %

Show Material materials with Iron of 62.65 - 100 %

Manganese

11.5 %

Show Material materials with Manganese of 11.5 %

Niobium

1 %

Show Material materials with Niobium of 1 %

Nitrogen

0.45 %

Show Material materials with Nitrogen of 0.45 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Tungsten

2 %

Show Material materials with Tungsten of 2 %

Vanadium

0.4 %

Show Material materials with Vanadium of 0.4 %