SAE J775 Grade XEV-D

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Reduction of area

20.0 °C

66 %

Show Material materials with Reduction of area of 66 %

760.0 °C

31 %

Show Material materials with Reduction of area of 31 %

Tensile strength

20.0 °C

800 MPa

Show Material materials with Tensile strength of 800 MPa

760.0 °C

320 MPa

Show Material materials with Tensile strength of 320 MPa

Unlock all property charts

Yield strength

20.0 °C

360 MPa

Show Material materials with Yield strength of 360 MPa

760.0 °C

170 MPa

Show Material materials with Yield strength of 170 MPa

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.55 %

Show Material materials with Carbon of 0.55 %

Chromium

21 %

Show Material materials with Chromium of 21 %

Iron

64.7 - 100 %

Show Material materials with Iron of 64.7 - 100 %

Manganese

8.25 %

Show Material materials with Manganese of 8.25 %

Nickel

2.8 %

Show Material materials with Nickel of 2.8 %

Nitrogen

0.45 %

Show Material materials with Nitrogen of 0.45 %

Silicon

0.15 %

Show Material materials with Silicon of 0.15 %

Tungsten

1.75 %

Show Material materials with Tungsten of 1.75 %

Vanadium

0.35 %

Show Material materials with Vanadium of 0.35 %