Chemical composition

Element Weight %
Fe 94.9049 — 96.3499
Cr 1.2 — 1.5
Al 0.95 — 1.3
Mn 0.7 — 0.95
C 0.35 — 0.4
Si 0.15 — 0.35
Mo 0.15 — 0.25
Se 0.15 — 0.25
S 0.0 — 0.06
P 0.0 — 0.035
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Download material data

Material data to download as .xlsx and .pdf file.

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFC22781 to find materials similar to AISI Nitriding B.