EN 12659 Grade Pb99.99

Want to keep this datasheet? Save it now in your required format

Description

Pb99,99 is a fine lead material for production of lead oxydes, pigments, accumulator plates, semi-finished part, alloys and corrosion resistant material for chemical instrument construction

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

11.34 g/cm³

Show Material materials with Density of 11.34 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

17 GPa

Show Material materials with Elastic modulus of 17 GPa

Poisson's ratio

23.0 °C

0.4 [-]

Show Material materials with Poisson's ratio of 0.4 [-]

Typical for Pure/Low Alloyed Lead

Tensile strength

20.0 °C

12.5 MPa

Show Material materials with Tensile strength of 12.5 MPa

Thermal

PropertyTemperatureValueComment

Melting point

327 °C

Show Material materials with Melting point of 327 °C

Typical for Pure/Low Alloyed Lead

Specific heat capacity

23.0 °C

112 - 134 J/(kg·K)

Show Material materials with Specific heat capacity of 112 - 134 J/(kg·K)

Typical for Pure/Low Alloyed Lead

Thermal conductivity

23.0 °C

34 - 35 W/(m·K)

Show Material materials with Thermal conductivity of 34 - 35 W/(m·K)

Typical for Pure/Low Alloyed Lead

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

2.07E-7 Ω·m

Show Material materials with Electrical resistivity of 2.07E-7 Ω·m

Chemical properties

PropertyValue

Antimony

1E-3 %

Show Material materials with Antimony of 1E-3 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

5E-3 %

Show Material materials with Bismuth of 5E-3 %

Copper

1E-3 %

Show Material materials with Copper of 1E-3 %

Iron

1E-3 %

Show Material materials with Iron of 1E-3 %

Lead

99.9 %

Show Material materials with Lead of 99.9 %

Silver

1E-3 %

Show Material materials with Silver of 1E-3 %

Tin

1E-3 %

Show Material materials with Tin of 1E-3 %

Zinc

1E-3 %

Show Material materials with Zinc of 1E-3 %