SEW 385 Grade Ni42 soft annealed (+A)

Want to keep this datasheet? Save it now in your required format

Description

The iron alloy with special thermal expansion Ni42, material number 1.3917, is used as chore material for copper-sheathed wire, expansion governors, IC flat casings, etched castings, alumina/ceramics compounds, transistor valves, as well as for bimetals (according to DIN 1715). The break point temperature (temperature at which a break point in the expansion-temperature-curve occurs) is 355 degrees C. The material has low thermal expansion at 300 degrees C. The cupping index at 1 mm thickness is 9.5 mm.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.2 g/cm³

Show Material materials with Density of 8.2 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

142 GPa

Show Material materials with Elastic modulus of 142 GPa

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Nickel Steel

Shear modulus

23.0 °C

76 GPa

Show Material materials with Shear modulus of 76 GPa

Typical for Nickel Steel

Tensile strength

20.0 °C

440 - 640 MPa

Show Material materials with Tensile strength of 440 - 640 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

5.6E-6 - 5.8E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.6E-6 - 5.8E-6 1/K

150.0 °C

5.5E-6 - 5.6E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.5E-6 - 5.6E-6 1/K

200.0 °C

5.4E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.4E-6 1/K

300.0 °C

5.4E-6 1/K

Show Material materials with Coefficient of thermal expansion of 5.4E-6 1/K

400.0 °C

6.2E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6.2E-6 1/K

500.0 °C

8.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 8.1E-6 1/K

600.0 °C

9.5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.5E-6 1/K

Melting point

1316 - 1595 °C

Show Material materials with Melting point of 1316 - 1595 °C

Typical for Nickel Steel

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

15 W/(m·K)

Show Material materials with Thermal conductivity of 15 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

6.2E-7 - 6.6E-7 Ω·m

Show Material materials with Electrical resistivity of 6.2E-7 - 6.6E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

40 - 43 %

Show Material materials with Nickel of 40 - 43 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %