Thermal
Property | Value | Comment |
---|---|---|
Melting point | 1480 °C Show Material materials with Melting point of 1480 °C | Typical for Ferrovanadium |
Chemical properties
Property | Value |
---|---|
Aluminium | 2 % Show Material materials with Aluminium of 2 % |
Carbon | 0.75 % Show Material materials with Carbon of 0.75 % |
Phosphorus | 0.08 % Show Material materials with Phosphorus of 0.08 % |
Silicon | 1.5 % Show Material materials with Silicon of 1.5 % |
Sulfur | 0.08 % Show Material materials with Sulfur of 0.08 % |
Vanadium | 75 - 85 % Show Material materials with Vanadium of 75 - 85 % |