EN AW-3003

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Electrical

Electrical conductivity σel

2.20E+7 - 2.90E+7 S/m at 20 °C

Electrical resistivity ρel

3.4E-8 - 4.5E-8 Ω·m at 20 °C

General

Density ρ

2.73 g/cm³ at 20 °C

Mechanical

Elastic modulus E

70 GPa at -270 °C

Show chart

Elongation A

10 - 70 % at 20 °C

Elongation A50 A50

4 - 6 % at 20 °C

Tensile strength Rm

20 - 280 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

10 - 230 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.15E-5 1/K at -50 °C

Show chart

Melting point Tm

654 - 655 °C

Specific heat capacity cp

892 - 893 J/(kg·K) at 20 °C

Thermal conductivity λ

160 - 200 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

96.7 - 98.95 %

Mn

1 - 1.5 %

Fe

0.7 %

Si

0.6 %

Zn

0.1 %

More

This material data has been provided by MetalInfo and AluKey and WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.