SAE SM-27

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Carbon

0.01 %

Show Material materials with Carbon of 0.01 %

Chromium

25 - 27.5 %

Show Material materials with Chromium of 25 - 27.5 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Manganese

0.4 %

Show Material materials with Manganese of 0.4 %

Molybdenum

0.75 - 1.5 %

Show Material materials with Molybdenum of 0.75 - 1.5 %

Nickel

0.5 %

Show Material materials with Nickel of 0.5 %

Niobium

0.05 - 0.2 %

Show Material materials with Niobium of 0.05 - 0.2 %

Nitrogen

0.02 %

Show Material materials with Nitrogen of 0.02 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

Sulfur

0.012 %

Show Material materials with Sulfur of 0.012 %