ISO 4957 Grade S 12-1-4-5 quenched (+Q)

Want to keep this datasheet? Save it now in your required format

Description

High V-Co alloyed top high speed steel with highest wear resistance, high hot hardness and tempering resistance. Application: face and scrub tools

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.12 g/cm³

Show Material materials with Density of 8.12 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

224 GPa

Show Material materials with Elastic modulus of 224 GPa

100.0 °C

220 GPa

Show Material materials with Elastic modulus of 220 GPa

200.0 °C

214 GPa

Show Material materials with Elastic modulus of 214 GPa

300.0 °C

207 GPa

Show Material materials with Elastic modulus of 207 GPa

400.0 °C

199 GPa

Show Material materials with Elastic modulus of 199 GPa

500.0 °C

191 GPa

Show Material materials with Elastic modulus of 191 GPa

600.0 °C

180 GPa

Show Material materials with Elastic modulus of 180 GPa

Poisson's ratio

20.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

Shear modulus

23.0 °C

79 GPa

Show Material materials with Shear modulus of 79 GPa

Typical for Tool And Machining Steel

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

9.6E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.6E-6 1/K

20.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

100.0 °C

1.11E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.11E-5 1/K

200.0 °C

1.16E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.16E-5 1/K

300.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

400.0 °C

1.24E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.24E-5 1/K

500.0 °C

1.27E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.27E-5 1/K

600.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

Unlock all property charts

Melting point

1370 - 1425 °C

Show Material materials with Melting point of 1370 - 1425 °C

Typical for Tool And Machining Steel

Specific heat capacity

23.0 °C

420 - 460 J/(kg·K)

Show Material materials with Specific heat capacity of 420 - 460 J/(kg·K)

Typical for Tool And Machining Steel

Thermal conductivity

20.0 °C

27.6 W/(m·K)

Show Material materials with Thermal conductivity of 27.6 W/(m·K)

100.0 °C

27.9 W/(m·K)

Show Material materials with Thermal conductivity of 27.9 W/(m·K)

200.0 °C

27.7 W/(m·K)

Show Material materials with Thermal conductivity of 27.7 W/(m·K)

300.0 °C

27.5 W/(m·K)

Show Material materials with Thermal conductivity of 27.5 W/(m·K)

400.0 °C

27 W/(m·K)

Show Material materials with Thermal conductivity of 27 W/(m·K)

500.0 °C

26.6 W/(m·K)

Show Material materials with Thermal conductivity of 26.6 W/(m·K)

600.0 °C

26.1 W/(m·K)

Show Material materials with Thermal conductivity of 26.1 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

5.24E-7 Ω·m

Show Material materials with Electrical resistivity of 5.24E-7 Ω·m

100.0 °C

5.81E-7 Ω·m

Show Material materials with Electrical resistivity of 5.81E-7 Ω·m

200.0 °C

6.64E-7 Ω·m

Show Material materials with Electrical resistivity of 6.64E-7 Ω·m

300.0 °C

7.51E-7 Ω·m

Show Material materials with Electrical resistivity of 7.51E-7 Ω·m

400.0 °C

8.44E-7 Ω·m

Show Material materials with Electrical resistivity of 8.44E-7 Ω·m

500.0 °C

9.41E-7 Ω·m

Show Material materials with Electrical resistivity of 9.41E-7 Ω·m

600.0 °C

1.04E-6 Ω·m

Show Material materials with Electrical resistivity of 1.04E-6 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

1.3 - 1.45 %

Show Material materials with Carbon of 1.3 - 1.45 %

Chromium

3.8 - 4.5 %

Show Material materials with Chromium of 3.8 - 4.5 %

Cobalt

4.5 - 5 %

Show Material materials with Cobalt of 4.5 - 5 %

Manganese

0.4 %

Show Material materials with Manganese of 0.4 %

Molybdenum

0.7 - 1 %

Show Material materials with Molybdenum of 0.7 - 1 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.45 %

Show Material materials with Silicon of 0.45 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

11.5 - 12.5 %

Show Material materials with Tungsten of 11.5 - 12.5 %

Vanadium

3.5 - 4 %

Show Material materials with Vanadium of 3.5 - 4 %