DIN 17480 Grade NiCr 20 TiAl solution heat-treated and precipitation hardened (+AT+P)

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.3 g/cm³

Show Material materials with Density of 8.3 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

215 GPa

Show Material materials with Elastic modulus of 215 GPa

Elongation

20.0 °C

15 %

Show Material materials with Elongation of 15 %

Hardness, Rockwell C

20.0 °C

32 [-]

Show Material materials with Hardness, Rockwell C of 32 [-]

Reduction of area

20.0 °C

25 %

Show Material materials with Reduction of area of 25 %

Tensile strength

20.0 °C

1100 - 1400 MPa

Show Material materials with Tensile strength of 1100 - 1400 MPa

500.0 °C

1050 MPa

Show Material materials with Tensile strength of 1050 MPa

550.0 °C

1030 MPa

Show Material materials with Tensile strength of 1030 MPa

600.0 °C

1000 MPa

Show Material materials with Tensile strength of 1000 MPa

650.0 °C

930 MPa

Show Material materials with Tensile strength of 930 MPa

700.0 °C

820 MPa

Show Material materials with Tensile strength of 820 MPa

750.0 °C

680 MPa

Show Material materials with Tensile strength of 680 MPa

800.0 °C

500 MPa

Show Material materials with Tensile strength of 500 MPa

Yield strength Rp0.2

20.0 °C

725 MPa

Show Material materials with Yield strength Rp0.2 of 725 MPa

500.0 °C

700 MPa

Show Material materials with Yield strength Rp0.2 of 700 MPa

550.0 °C

650 MPa

Show Material materials with Yield strength Rp0.2 of 650 MPa

600.0 °C

650 MPa

Show Material materials with Yield strength Rp0.2 of 650 MPa

650.0 °C

600 MPa

Show Material materials with Yield strength Rp0.2 of 600 MPa

700.0 °C

600 MPa

Show Material materials with Yield strength Rp0.2 of 600 MPa

750.0 °C

500 MPa

Show Material materials with Yield strength Rp0.2 of 500 MPa

800.0 °C

450 MPa

Show Material materials with Yield strength Rp0.2 of 450 MPa

Unlock all property charts

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.19E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K

300.0 °C

1.31E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.31E-5 1/K

500.0 °C

1.37E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.37E-5 1/K

700.0 °C

1.45E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.45E-5 1/K

Unlock all property charts

Max service temperature, long

0 - 1000 °C

Show Material materials with Max service temperature, long of 0 - 1000 °C

Specific heat capacity

20.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

20.0 °C

13 W/(m·K)

Show Material materials with Thermal conductivity of 13 W/(m·K)

Chemical properties

PropertyValue

Aluminium

1 - 1.8 %

Show Material materials with Aluminium of 1 - 1.8 %

Boron

8E-3 %

Show Material materials with Boron of 8E-3 %

Carbon

0.04 - 0.1 %

Show Material materials with Carbon of 0.04 - 0.1 %

Chromium

18 - 21 %

Show Material materials with Chromium of 18 - 21 %

Cobalt

2 %

Show Material materials with Cobalt of 2 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Iron

1.5 %

Show Material materials with Iron of 1.5 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

1.8 - 2.7 %

Show Material materials with Titanium of 1.8 - 2.7 %