EN S500MLO

Want to keep this datasheet? Save it now in your required format

Description

Weldable structural steels for stationary offshore structures.

Related Standards

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.85 g/cm³

Show Material materials with Density of 7.85 g/cm³

Mechanical

PropertyTemperatureValueComment

Charpy impact energy, V-notch

-40.0 °C

60 J

Show Material materials with Charpy impact energy, V-notch of 60 J

Elongation

23.0 °C

15 %

Show Material materials with Elongation of 15 %

min.

Tensile strength

23.0 °C

540 - 740 MPa

Show Material materials with Tensile strength of 540 - 740 MPa

Yield strength

23.0 °C

440 - 500 MPa

Show Material materials with Yield strength of 440 - 500 MPa

min., depending on the thickness, If not apparent, the yield strength Rp0.2 is measured

Chemical properties

PropertyValueComment

Aluminium

0.015 - 0.055 %

Show Material materials with Aluminium of 0.015 - 0.055 %

Carbon

0.14 %

Show Material materials with Carbon of 0.14 %

max.

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

max.

Copper

0.35 %

Show Material materials with Copper of 0.35 %

max.

Manganese

2 %

Show Material materials with Manganese of 2 %

max.

Molybdenum

0.25 %

Show Material materials with Molybdenum of 0.25 %

max.

Nickel

1 %

Show Material materials with Nickel of 1 %

max.

Niobium

0.05 %

Show Material materials with Niobium of 0.05 %

max.

Nitrogen

0.01 %

Show Material materials with Nitrogen of 0.01 %

max.

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

max.

Silicon

0.55 %

Show Material materials with Silicon of 0.55 %

max.

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

max.

Titanium

0.03 %

Show Material materials with Titanium of 0.03 %

max.

Vanadium

0.08 %

Show Material materials with Vanadium of 0.08 %

max.

Technological properties

Property

International welding carbon equivalent

0.47 [-]

max., if Nb + V <0.12%

Other

The level of residual elements of arsenic, antimony, tin, lead, bismuth, calcium and boron should not exceed 0.03% As, 0.010% Sb, 0.020% Sn, 0.010% Pb, 0.010% Bi, 0.005% Ca and 0.0008% B