ASTM B763 Grade C95400 HT, Heat-Treated; Separately Cast Test Bars

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A50

20.0 °C

6 %

Show Material materials with Elongation A50 of 6 %

Hardness, Brinell

20.0 °C

190 [-]

Show Material materials with Hardness, Brinell of 190 [-]

Tensile strength

20.0 °C

620 MPa

Show Material materials with Tensile strength of 620 MPa

Yield strength Rp0.5

20.0 °C

310 MPa

Show Material materials with Yield strength Rp0.5 of 310 MPa

Chemical properties

PropertyValue

Aluminium

10 - 11.5 %

Show Material materials with Aluminium of 10 - 11.5 %

Copper

83 %

Show Material materials with Copper of 83 %

Iron

3 - 5 %

Show Material materials with Iron of 3 - 5 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Nickel

1.5 %

Show Material materials with Nickel of 1.5 %