Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 6 % Show Material materials with Elongation A50 of 6 % |
Hardness, Brinell | 20.0 °C | 190 [-] Show Material materials with Hardness, Brinell of 190 [-] |
Tensile strength | 20.0 °C | 620 MPa Show Material materials with Tensile strength of 620 MPa |
Yield strength Rp0.5 | 20.0 °C | 310 MPa Show Material materials with Yield strength Rp0.5 of 310 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 11.5 % Show Material materials with Aluminium of 10 - 11.5 % |
Copper | 83 % Show Material materials with Copper of 83 % |
Iron | 3 - 5 % Show Material materials with Iron of 3 - 5 % |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % |
Nickel | 1.5 - 2.5 % Show Material materials with Nickel of 1.5 - 2.5 % |