Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 5 % Show Material materials with Elongation A50 of 5 % |
Hardness, Brinell | 20.0 °C | 200 [-] Show Material materials with Hardness, Brinell of 200 [-] |
Tensile strength | 20.0 °C | 760 MPa Show Material materials with Tensile strength of 760 MPa |
Yield strength Rp0.5 | 20.0 °C | 415 MPa Show Material materials with Yield strength Rp0.5 of 415 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 11.5 % Show Material materials with Aluminium of 10 - 11.5 % |
Copper | 78 % Show Material materials with Copper of 78 % |
Iron | 3 - 5 % Show Material materials with Iron of 3 - 5 % |
Manganese | 3.5 % Show Material materials with Manganese of 3.5 % |
Nickel | 3 - 5.5 % Show Material materials with Nickel of 3 - 5.5 % |