Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 100 - 125 GPa Show Material materials with Elastic modulus of 100 - 125 GPa | Typical for Wrought Copper Brass |
Elongation | 23.0 °C | 43 % Show Material materials with Elongation of 43 % | |
Shear modulus | 23.0 °C | 40 GPa Show Material materials with Shear modulus of 40 GPa | Typical for Wrought Copper Brass |
Tensile strength | 23.0 °C | 285 - 340 MPa Show Material materials with Tensile strength of 285 - 340 MPa | |
Yield strength Rp0.2 | 23.0 °C | 85 MPa Show Material materials with Yield strength Rp0.2 of 85 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Melting point | 875 - 1075 °C Show Material materials with Melting point of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Thermal conductivity | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Thermal conductivity of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Copper | 86 - 89 % Show Material materials with Copper of 86 - 89 % |
Iron | 0.05 % Show Material materials with Iron of 0.05 % |
Lead | 0.05 % Show Material materials with Lead of 0.05 % |
Phosphorus | 0.35 % Show Material materials with Phosphorus of 0.35 % |
Tin | 0.8 - 1.4 % Show Material materials with Tin of 0.8 - 1.4 % |
Do you have a technical question or need more information about this material?
Post it as a comment below and receive answers from engineers and other community members.