Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Density of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Elongation | 23.0 °C | 10 % Show Material materials with Elongation of 10 % | |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 23.0 °C | 470 - 545 MPa Show Material materials with Tensile strength of 470 - 545 MPa | |
Yield strength Rp0.2 | 23.0 °C | 420 MPa Show Material materials with Yield strength Rp0.2 of 420 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Specific heat capacity | 23.0 °C | 380 J/(kg·K) Show Material materials with Specific heat capacity of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Lead | 0.05 % Show Material materials with Lead of 0.05 % |
Phosphorus | 0.03 - 0.35 % Show Material materials with Phosphorus of 0.03 - 0.35 % |
Tin | 4.2 - 5.8 % Show Material materials with Tin of 4.2 - 5.8 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |