General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 2.72 g/cm³ Show Material materials with Density of 2.72 g/cm³ | Typical for Cast Aluminium Manganese Grade |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 40 - 45 GPa Show Material materials with Elastic modulus of 40 - 45 GPa | Typical for Cast Aluminium Manganese Grade |
Elongation A50 | 23.0 °C | 10 % Show Material materials with Elongation A50 of 10 % | |
Hardness, Brinell | 23.0 °C | 58 [-] Show Material materials with Hardness, Brinell of 58 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Magnesium |
Shear modulus | 23.0 °C | 45 GPa Show Material materials with Shear modulus of 45 GPa | Typical for Magnesium |
Tensile strength | 23.0 °C | 200 MPa Show Material materials with Tensile strength of 200 MPa | |
Yield strength | 23.0 °C | 110 MPa Show Material materials with Yield strength of 110 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.5E-5 - 2.6E-5 1/K | Typical for Cast Aluminium Manganese Grade |
Melting point | 465 - 620 °C Show Material materials with Melting point of 465 - 620 °C | Typical for Cast Aluminium Manganese Grade | |
Specific heat capacity | 23.0 °C | 1000 - 1080 J/(kg·K) Show Material materials with Specific heat capacity of 1000 - 1080 J/(kg·K) | Typical for Cast Aluminium Manganese Grade |
Thermal conductivity | 23.0 °C | 42 - 75 W/(m·K) Show Material materials with Thermal conductivity of 42 - 75 W/(m·K) | Typical for Cast Aluminium Manganese Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 4.4 - 5.4 % Show Material materials with Aluminium of 4.4 - 5.4 % |
Copper | 0.01 % Show Material materials with Copper of 0.01 % |
Iron | 4E-3 % Show Material materials with Iron of 4E-3 % |
Manganese | 0.26 - 0.6 % Show Material materials with Manganese of 0.26 - 0.6 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |
Zinc | 0.22 % Show Material materials with Zinc of 0.22 % |