Elongation A50 A50
0 - 7 % at 20 °C
Hardness, Brinell HB
55 [-] at 20 °C
Tensile strength Rm
0 - 234 MPa at 20 °C
Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_
0 - 76 MPa at 20 °C
Element
Weight %
Comment
7 - 8.1 %
0.4 - 1 %
0.13 - 0.35 %
0 - 0.1 %
0 - 0.01 %