Description

Related Standards

Properties

Mechanical

Elongation A50 A50

2 % at 20 °C

Hardness, Brinell HB

62 [-] at 20 °C

Tensile strength Rm

158 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

83 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Al

8.1 - 9.3 %

Zn

0.4 - 1 %

Si

0.3 %

Mn

0.13 - 0.35 %

Cu

0.1 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.