ASTM B199 Grade AZ92A F

Want to keep this datasheet? Save it now in your required format

Description

Related Standards

Properties

Mechanical

Hardness, Brinell

HB

65 [-] at 20 °C

Tensile strength

Rm

158 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

76 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Al

8.3 - 9.7 %

Zn

1.6 - 2.4 %

Si

0.3 %

Cu

0.25 %

Mn

0.1 - 0.35 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.