Mechanical

Hardness, Brinell HB

81 [-] at 20 °C

Tensile strength Rm

234 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

124 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Al

8.3 - 9.7 %

Zn

1.6 - 2.4 %

Si

0.3 %

Cu

0.25 %

Mn

0.1 - 0.35 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.