Elongation A
0 - 4 % at 20 °C
Tensile strength Rm
0 - 455 MPa at 20 °C
Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_
0 - 400 MPa at 20 °C
Element
Weight %
Comment
3.8 - 4.9 %
1.2 - 1.8 %
0.3 - 0.9 %
0 - 0.1 %
0 - 0.5 %
This material data has been provided by ASTM.