This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Tensile strength Rm
0 - 150 MPa at 20 °C
Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_
0 - 130 MPa at 20 °C
Element
Weight %
Comment
1 - 1.5 %
0.05 - 0.2 %
0 - 0.7 %
0 - 0.6 %
0 - 0.1 %
This material data has been provided by ASTM.