Tensile strength Rm
0 - 215 MPa at 20 °C
Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_
0 - 160 MPa at 20 °C
Element
Weight %
Comment
2.2 - 2.8 %
0.15 - 0.35 %
0 - 0.1 %
0 - 0.4 %
0 - 0.1 %
This material data has been provided by ASTM.