Elongation A50 A50
0 - 8 % at 20 °C
Tensile strength Rm
0 - 260 MPa at 20 °C
Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_
0 - 240 MPa at 20 °C
Element
Weight %
Comment
0.8 - 1.2 %
0.4 - 0.8 %
0.15 - 0.4 %
0.04 - 0.35 %
0 - 0.7 %
This material data has been provided by ASTM.