AIR 9160 Grade 9160C231 solution treated and tempered bar

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Tensile strength Rm

960 MPa at 20 °C

Yield strength YS

660 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

49.22 - 58.1 %

Ni

24 - 27 %

Cr

13.5 - 16 %

Ti

1.9 - 2.3 %

Mn

1 - 2 %

More

Technological properties

Processing history

solution treated and tempered

This material data has been provided by MetalInfo.