Wrought Aluminium

EN AW-1050A F Rod

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Electrical

Electrical conductivity σel

0 - 3.60E+7 S/m at 20 °C

Electrical resistivity ρel

2.8E-8 - 2.9E-8 Ω·m at 20 °C

General

Density ρ

2.7 - 2.71 g/cm³ at 20 °C

Mechanical

Elastic modulus E

70 GPa at -270 °C

Show chart

Elongation A

25 % at 20 °C

Elongation A50 A50

23 % at 20 °C

Tensile strength Rm

60 - 130 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

20 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.17E-5 1/K at -50 °C

Show chart

Melting point Tm

657 - 658 °C

Specific heat capacity cp

899 - 900 J/(kg·K) at 20 °C

Thermal conductivity λ

210 - 229 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

99.5 - 99.98 %

Fe

0.4 %

Si

0.1 - 0.25 %

Cu

0.05 %

B

0.05 %

More

Technological properties

Processing history

casting,hot-rolled,

This material data has been provided by MetalInfo and WIAM.