Mechanical

Tensile strength Rm

180 - 240 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Al

90.5 - 94.7 %

Cu

3.8 - 4.9 %

Mg

1.2 - 1.8 %

Si

0.5 %

Fe

0.5 %