Customize your search with filters
Do you have any questions?
Electrical conductivity σel
1.80E+7 - 2.80E+7 S/m at 20 °C
Density ρ
2.79 - 2.8 g/cm³ at 20 °C
Elastic modulus E
65 - 73.5 GPa at 20 °C
Elongation A
2 - 12 % at 20 °C
Elongation A5 A5
4 - 12 % at 20 °C
Elongation A50 A50
13 - 15 % at 20 °C
Hardness, Brinell HB
101 - 111 [-] at 20 °C
Tensile strength Rm
300 - 390 MPa at 20 °C
Yield strength Rp0.2 Rp0.2
200 - 260 MPa at 20 °C
Melting point Tm
650 °C
Specific heat capacity cp
921 J/(kg·K) at 20 °C
Thermal conductivity λ
130 - 200 W/(m·K) at 20 °C
Element
Weight %
Comment
91.2 - 95.5 %
3.5 - 4.5 %
0.7 %
0.4 - 1 %
0.4 - 1 %
This material data has been provided by MetalInfo and WIAM.