EN AW-2024 T351 Flat

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Electrical

Electrical conductivity σel

1.60E+7 - 2.10E+7 S/m at 20 °C

General

Density ρ

2.77 - 2.78 g/cm³ at 20 °C

Mechanical

Elastic modulus E

70 - 74.5 GPa at 20 °C

Elongation A

5 - 11 % at 20 °C

Elongation A5 A5

5 - 11 % at 20 °C

Elongation A50 A50

12 - 14 % at 20 °C

Hardness, Brinell HB

104 - 124 [-] at 20 °C

Tensile strength Rm

360 - 440 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

250 - 290 MPa at 20 °C

Thermal

Melting point Tm

640 °C

Specific heat capacity cp

875 J/(kg·K) at 20 °C

Thermal conductivity λ

130 - 150 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

90.5 - 94.7 %

Cu

3.8 - 4.9 %

Mg

1.2 - 1.8 %

Si

0.5 %

Fe

0.5 %

More

This material data has been provided by MetalInfo and WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.