Customize your search with filters
Do you have any questions?
Electrical conductivity σel
1.60E+7 - 2.10E+7 S/m at 20 °C
Density ρ
2.77 - 2.78 g/cm³ at 20 °C
Elastic modulus E
70 - 74.5 GPa at 20 °C
Elongation A
8 % at 20 °C
Elongation A5 A5
8 - 12 % at 20 °C
Elongation A50 A50
6 - 10 % at 20 °C
Tensile strength Rm
240 - 440 MPa at 20 °C
Yield strength Rp0.2 Rp0.2
140 - 290 MPa at 20 °C
Melting point Tm
640 °C
Specific heat capacity cp
875 J/(kg·K) at 20 °C
Thermal conductivity λ
130 - 150 W/(m·K) at 20 °C
Element
Weight %
Comment
90.5 - 94.7 %
3.8 - 4.9 %
1.2 - 1.8 %
0.5 %
0.5 %
This material data has been provided by MetalInfo and WIAM.