Do you have any questions?
Electrical conductivity σel
18 S/m at 20 °C
Electrical resistivity ρel
0.04 Ω·m at 20 °C
Density ρ
2.8 g/cm³ at 20 °C
Elastic modulus E
72.5 GPa at 20 °C
Elongation A5 A5
12 % at 20 °C
Elongation A50 A50
10 - 14 % at 20 °C
Hardness, Brinell HB
55 [-] at 20 °C
Tensile strength Rm
150 - 250 MPa at 20 °C
Yield strength Rp0.2 Rp0.2
135 MPa at 20 °C
Melting point Tm
512 °C
Thermal conductivity λ
130 W/(m·K) at 20 °C
Element
Weight %
Comment
91.2 - 95.5 %
3.5 - 4.5 %
0.7 %
0.4 - 1 %
0.4 - 1 %
This material data has been provided by MetalInfo and AluKey.