Properties

Electrical

Electrical conductivity σel

18 - 2.80E+7 S/m at 20 °C

Electrical resistivity ρel

0.04 Ω·m at 20 °C

General

Density ρ

2.79 - 2.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

65 - 73.5 GPa at 20 °C

Elongation A

12 % at 20 °C

Elongation A5 A5

10 - 12 % at 20 °C

Elongation A50 A50

8 - 14 % at 20 °C

Hardness, Brinell HB

55 [-] at 20 °C

Tensile strength Rm

150 - 400 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

135 - 270 MPa at 20 °C

Thermal

Melting point Tm

512 - 650 °C

Specific heat capacity cp

921 J/(kg·K) at 20 °C

Thermal conductivity λ

130 - 200 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

91.2 - 95.5 %

Cu

3.5 - 4.5 %

Fe

0.7 %

Mg

0.4 - 1 %

Mn

0.4 - 1 %

More

This material data has been provided by MetalInfo and AluKey and WIAM.