Elongation A5 A5
10 % at 20 °C
Elongation A50 A50
8 % at 20 °C
Tensile strength Rm
380 MPa at 20 °C
Yield strength Rp0.2 Rp0.2
260 MPa at 20 °C
Element
Weight %
Comment
91.2 - 95.5 %
3.5 - 4.5 %
0.7 %
0.4 - 1 %
0.4 - 1 %
This material data has been provided by MetalInfo.