EN 573-1 Grade AW-3003 H19

Want to keep this datasheet? Save it now in your required format

Description

Good combination of resistance to corrosion, weldability and formability.

Related Standards

Equivalent Materials

Ashby charts

See where EN 573-1 Grade AW-3003 H19 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.73 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.2 - 2 mm

Mechanical

Plane-Strain Fracture Toughnes

KIC

Typical for Wrought 3000 Series Aluminium

Yield strength Rp0.2, transverse

Rp0.2,trans

Thermal

Coefficient of thermal expansion

α

2.15E-5 1/K at -50 °C

20-100°C

Unlock all property charts

Melting point

Tm

640 - 655 °C

Specific heat capacity

cp

892 - 893 J/(kg·K) at 20 °C

Thermal conductivity

λ

159 - 200 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

2.20E+7 - 2.90E+7 S/m at 20 °C

Electrical resistivity

ρel

3.4E-8 - 4.5E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Mn

1 - 1.5 %

Fe

0.7 %

Si

0.6 %

Zn

0.1 %

More

Technological properties

Anodizing

Good

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Anodizing Quality; Electronic devices: Housing of devices; Heat exchangers: Fins, Heat exchangers, General appliacations; Tubes: Industrial tubes, Flexible tube, Pipes; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetics pieces; Semi-rigid and corrugated: Smooth wall; Automotive trim: Interior trims; Components: Heat shields, Automotive fins, Heat exchangers, General transportation

Brazing

Excellent

Corrosion properties

Very Good

Welding

Very Good

Workability

Very Good

This material data has been provided by Aludium,WIAM,AluKey.