DIN 1681 Grade GS-38 heat treated

Want to keep this datasheet? Save it now in your required format

Description

GS-38, for castings without special stress: application in the mechanical engineering, in the manufacturing of vehicles and materials handling equipment, e.g. hubs, bushes, lids, casings. For castings, for static or dynamic stress with good welding properties, e.g. welded hubs, bearing bodies, mount-arm assemblies, bearing end plates. With higher static or dynamic stress for spoke wheel centres, brake block shoes, roller-bearing type axle box casings. Application for temperatures between -10 and +300 °C.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.85 g/cm³

Show Material materials with Density of 7.85 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

194 GPa

Show Material materials with Elastic modulus of 194 GPa

Elongation

20.0 °C

25 %

Show Material materials with Elongation of 25 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Reduction of area

20.0 °C

40 %

Show Material materials with Reduction of area of 40 %

Shear modulus

23.0 °C

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Tensile strength

20.0 °C

380 MPa

Show Material materials with Tensile strength of 380 MPa

Yield strength

20.0 °C

200 MPa

Show Material materials with Yield strength of 200 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Max service temperature, long

-10 - 300 °C

Show Material materials with Max service temperature, long of -10 - 300 °C

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

20.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

20.0 °C

57 W/(m·K)

Show Material materials with Thermal conductivity of 57 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

0.25 %

Show Material materials with Carbon of 0.25 %

Do you have a technical question or need more information about this material?