General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Density | 20.0 °C | 2.68 g/cm³ Show Material materials with Density of 2.68 g/cm³ | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 72.0 Show Material materials with Elastic modulus of 72.0 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | |
Elongation | -196.0 °C | 28.0 % Show Material materials with Elongation of 28.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | |
-80.0 °C | 21.0 % Show Material materials with Elongation of 21.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
-28.0 °C | 18.0 % Show Material materials with Elongation of 18.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
20.0 °C | 16.0 % Show Material materials with Elongation of 16.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
100.0 °C | 18.0 % Show Material materials with Elongation of 18.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
150.0 °C | 27.0 % Show Material materials with Elongation of 27.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
200.0 °C | 45.0 % Show Material materials with Elongation of 45.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
260.0 °C | 80.0 % Show Material materials with Elongation of 80.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
315.0 °C | 110.0 % Show Material materials with Elongation of 110.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
370.0 °C | 130.0 % Show Material materials with Elongation of 130.0 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | |||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | |||
Shear modulus | 20.0 °C | 27.0 Show Material materials with Shear modulus of 27.0 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | |
Tensile strength | -196.0 °C | 380.0 MPa Show Material materials with Tensile strength of 380.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | |
-80.0 °C | 280.0 MPa Show Material materials with Tensile strength of 280.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
-28.0 °C | 260.0 MPa Show Material materials with Tensile strength of 260.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
20.0 °C | 260.0 MPa Show Material materials with Tensile strength of 260.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
100.0 °C | 260.0 MPa Show Material materials with Tensile strength of 260.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
150.0 °C | 205.0 MPa Show Material materials with Tensile strength of 205.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
200.0 °C | 165.0 MPa Show Material materials with Tensile strength of 165.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
260.0 °C | 85.0 MPa Show Material materials with Tensile strength of 85.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
315.0 °C | 50.0 MPa Show Material materials with Tensile strength of 50.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
370.0 °C | 35.0 MPa Show Material materials with Tensile strength of 35.0 MPa | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | -50.0 °C | 2.21e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.21e-05 1/K | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | |
100.0 °C | 2.38e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
200.0 °C | 2.48e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.48e-05 1/K | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
300.0 °C | 2.57e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.57e-05 1/K | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | ||
Max service temperature | 150.0 °C Show Material materials with Max service temperature of 150.0 °C | Typical for Wrought 5000 Series Aluminium | |||
Melting point | 560.0 - 655.0 °C Show Material materials with Melting point of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | |||
Specific heat capacity | 20.0 °C | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | |
Thermal conductivity | 20.0 °C | 150.0 Show Material materials with Thermal conductivity of 150.0 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Electrical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 21000000.0 Show Material materials with Electrical conductivity of 21000000.0 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 | |
Electrical resistivity | 3.3e-08 - 5e-08 Ω·m Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Chromium | 0.15 - 0.35 % Show Material materials with Chromium of 0.15 - 0.35 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Copper | 0.1 Show Material materials with Copper of 0.1 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Iron | 0.4 Show Material materials with Iron of 0.4 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Magnesium | 2.2 - 2.8 % Show Material materials with Magnesium of 2.2 - 2.8 % | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Manganese | 0.1 Show Material materials with Manganese of 0.1 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Silicon | 0.25 Show Material materials with Silicon of 0.25 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | G25 | DIN 1725-1, EN 573-3, EN 573-4, WL 3.3524-1 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |
Do you have a technical question or need more information about this material?
Post it as a comment below and receive answers from engineers and other community members.