EN 10210-1 Grade S460NH hot finished

Want to keep this datasheet? Save it now in your required format

Description

Hot finished weldable structural hollow sections with circular, square, rectangular or elliptical cross-section for the steel and plant construction, civil engineering and vehicle construction.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

540 - 720 MPa

Show Material materials with Tensile strength of 540 - 720 MPa

Yield strength

20.0 °C

430 - 460 MPa

Show Material materials with Yield strength of 430 - 460 MPa

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Carbon

0.22 %

Show Material materials with Carbon of 0.22 %

Chromium

0.3 %

Show Material materials with Chromium of 0.3 %

Copper

0.7 %

Show Material materials with Copper of 0.7 %

Manganese

1 - 1.7 %

Show Material materials with Manganese of 1 - 1.7 %

Molybdenum

0.1 %

Show Material materials with Molybdenum of 0.1 %

Nickel

0.8 %

Show Material materials with Nickel of 0.8 %

Niobium

0.05 %

Show Material materials with Niobium of 0.05 %

Nitrogen

0.03 %

Show Material materials with Nitrogen of 0.03 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Titanium

0.03 %

Show Material materials with Titanium of 0.03 %

Vanadium

0.2 %

Show Material materials with Vanadium of 0.2 %