Description

Fully austenitic steel of high scaling temp. of 1150°C in air (highest application temp. in air), warranted scaling resistance for wide and fast thermal fluctuation, but no resistance in reducing athmosphere. Excellent creep behaviour and high deformation resistance. Application for furnace components, hood annealing and muffle furnaces, lifting bar furnaces, sealing sheets, radiator tubes, charging cages, insert boxes, recuperators as well as for combustion nozzles and for strongly loaded components of waste gas detoxification facilities.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

Typical for Austenitic Stainless Steel

Elongation

20.0 °C

40 %

Show Material materials with Elongation of 40 %

Elongation A80

20.0 °C

37 %

Show Material materials with Elongation A80 of 37 %

Hardness, Brinell

20.0 °C

210 [-]

Show Material materials with Hardness, Brinell of 210 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Tensile strength

20.0 °C

650 - 850 MPa

Show Material materials with Tensile strength of 650 - 850 MPa

Yield strength Rp0.2

20.0 °C

310 MPa

Show Material materials with Yield strength Rp0.2 of 310 MPa

Yield strength Rp1.0

20.0 °C

350 MPa

Show Material materials with Yield strength Rp1.0 of 350 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

200.0 °C

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

400.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

600.0 °C

1.85E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.85E-5 1/K

800.0 °C

1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.9E-5 1/K

1000.0 °C

1.95E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.95E-5 1/K

Max service temperature, long

0 - 1150 °C

Show Material materials with Max service temperature, long of 0 - 1150 °C

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

600.0 °C

660 J/(kg·K)

Show Material materials with Specific heat capacity of 660 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

15 W/(m·K)

Show Material materials with Thermal conductivity of 15 W/(m·K)

500.0 °C

21 W/(m·K)

Show Material materials with Thermal conductivity of 21 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

8.5E-7 Ω·m

Show Material materials with Electrical resistivity of 8.5E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.05 - 0.12 %

Show Material materials with Carbon of 0.05 - 0.12 %

Cerium

0.03 - 0.08 %

Show Material materials with Cerium of 0.03 - 0.08 %

Chromium

20 - 22 %

Show Material materials with Chromium of 20 - 22 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

10 - 12 %

Show Material materials with Nickel of 10 - 12 %

Nitrogen

0.12 - 0.2 %

Show Material materials with Nitrogen of 0.12 - 0.2 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1.4 - 2.5 %

Show Material materials with Silicon of 1.4 - 2.5 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %