EN 10222-3 Grade X8Ni9 normalized or quenched and tempered

Want to keep this datasheet? Save it now in your required format

Description

The nickel-alloyed cryogenic material X8Ni9, materia number 1.5662 is used in pressure vessel construction. Application for refrigerators, gearbox parts and components in machine and apparatus engineering which are exposed to temperatures up to -200 °C.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.88 g/cm³

Show Material materials with Density of 7.88 g/cm³

27.0 °C

7.84 g/cm³

Show Material materials with Density of 7.84 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

-269.0 °C

205.5 GPa

Show Material materials with Elastic modulus of 205.5 GPa

-200.0 °C

205.2 GPa

Show Material materials with Elastic modulus of 205.2 GPa

-150.0 °C

203.4 GPa

Show Material materials with Elastic modulus of 203.4 GPa

-100.0 °C

201 - 201.4 GPa

Show Material materials with Elastic modulus of 201 - 201.4 GPa

-50.0 °C

198.9 GPa

Show Material materials with Elastic modulus of 198.9 GPa

20.0 °C

195 GPa

Show Material materials with Elastic modulus of 195 GPa

27.0 °C

195.1 GPa

Show Material materials with Elastic modulus of 195.1 GPa

100.0 °C

190 GPa

Show Material materials with Elastic modulus of 190 GPa

200.0 °C

184 GPa

Show Material materials with Elastic modulus of 184 GPa

300.0 °C

178 GPa

Show Material materials with Elastic modulus of 178 GPa

400.0 °C

170 GPa

Show Material materials with Elastic modulus of 170 GPa

Unlock all property charts

Poisson's ratio

-269.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

-200.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

-150.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

-100.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

-50.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

27.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Unlock all property charts

Shear modulus

-269.0 °C

80 GPa

Show Material materials with Shear modulus of 80 GPa

-200.0 °C

79.8 GPa

Show Material materials with Shear modulus of 79.8 GPa

-150.0 °C

79 GPa

Show Material materials with Shear modulus of 79 GPa

-100.0 °C

78.2 GPa

Show Material materials with Shear modulus of 78.2 GPa

-50.0 °C

77.1 GPa

Show Material materials with Shear modulus of 77.1 GPa

27.0 °C

75.4 GPa

Show Material materials with Shear modulus of 75.4 GPa

Unlock all property charts

Yield strength Rp0.2

100.0 °C

370 MPa

Show Material materials with Yield strength Rp0.2 of 370 MPa

200.0 °C

335 MPa

Show Material materials with Yield strength Rp0.2 of 335 MPa

250.0 °C

315 MPa

Show Material materials with Yield strength Rp0.2 of 315 MPa

300.0 °C

300 MPa

Show Material materials with Yield strength Rp0.2 of 300 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

1.02E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

20.0 °C

1.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K

100.0 °C

1.14E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.14E-5 1/K

200.0 °C

1.18E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.18E-5 1/K

300.0 °C

1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K

400.0 °C

1.25E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.25E-5 1/K

Unlock all property charts

Melting point

1316 - 1595 °C

Show Material materials with Melting point of 1316 - 1595 °C

Typical for Nickel Steel

Specific heat capacity

-100.0 °C

442 J/(kg·K)

Show Material materials with Specific heat capacity of 442 J/(kg·K)

20.0 °C

464 J/(kg·K)

Show Material materials with Specific heat capacity of 464 J/(kg·K)

100.0 °C

479 J/(kg·K)

Show Material materials with Specific heat capacity of 479 J/(kg·K)

200.0 °C

495 J/(kg·K)

Show Material materials with Specific heat capacity of 495 J/(kg·K)

300.0 °C

511 J/(kg·K)

Show Material materials with Specific heat capacity of 511 J/(kg·K)

400.0 °C

528 J/(kg·K)

Show Material materials with Specific heat capacity of 528 J/(kg·K)

Unlock all property charts

Thermal conductivity

-100.0 °C

23.9 W/(m·K)

Show Material materials with Thermal conductivity of 23.9 W/(m·K)

20.0 °C

30.2 W/(m·K)

Show Material materials with Thermal conductivity of 30.2 W/(m·K)

100.0 °C

32.8 W/(m·K)

Show Material materials with Thermal conductivity of 32.8 W/(m·K)

200.0 °C

34.4 W/(m·K)

Show Material materials with Thermal conductivity of 34.4 W/(m·K)

300.0 °C

34.7 W/(m·K)

Show Material materials with Thermal conductivity of 34.7 W/(m·K)

400.0 °C

34 W/(m·K)

Show Material materials with Thermal conductivity of 34 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

8.3 mm²/s

Show Material materials with Thermal diffusivity of 8.3 mm²/s

100.0 °C

8.5 mm²/s

Show Material materials with Thermal diffusivity of 8.5 mm²/s

200.0 °C

8.4 mm²/s

Show Material materials with Thermal diffusivity of 8.4 mm²/s

300.0 °C

8 mm²/s

Show Material materials with Thermal diffusivity of 8 mm²/s

400.0 °C

7.3 mm²/s

Show Material materials with Thermal diffusivity of 7.3 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

-100.0 °C

2.51E-7 Ω·m

Show Material materials with Electrical resistivity of 2.51E-7 Ω·m

20.0 °C

3.22E-7 Ω·m

Show Material materials with Electrical resistivity of 3.22E-7 Ω·m

100.0 °C

3.73E-7 Ω·m

Show Material materials with Electrical resistivity of 3.73E-7 Ω·m

200.0 °C

4.4E-7 Ω·m

Show Material materials with Electrical resistivity of 4.4E-7 Ω·m

300.0 °C

5.19E-7 Ω·m

Show Material materials with Electrical resistivity of 5.19E-7 Ω·m

400.0 °C

6.13E-7 Ω·m

Show Material materials with Electrical resistivity of 6.13E-7 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Manganese

0.3 - 0.8 %

Show Material materials with Manganese of 0.3 - 0.8 %

Molybdenum

0.1 %

Show Material materials with Molybdenum of 0.1 %

Nickel

8.5 - 10 %

Show Material materials with Nickel of 8.5 - 10 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.35 %

Show Material materials with Silicon of 0.35 %

Sulfur

0.005 - 0.01 %

Show Material materials with Sulfur of 0.005 - 0.01 %

Vanadium

0.05 %

Show Material materials with Vanadium of 0.05 %