EN 10137-2 Grade S620Q quenched and tempered (+QT)

Want to keep this datasheet? Save it now in your required format

Description

The tempered and fine grain weldable steel S620Q is used for constructions, such as transport vehicles, lifting and earthmoving machines, load-carrying constructions etc. Lowest application temperature -20 °C.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.84 g/cm³

Show Material materials with Density of 7.84 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

Elongation

20.0 °C

15 %

Show Material materials with Elongation of 15 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Shear modulus

20.0 °C

80 GPa

Show Material materials with Shear modulus of 80 GPa

Tensile strength

20.0 °C

650 - 890 MPa

Show Material materials with Tensile strength of 650 - 890 MPa

Yield strength

20.0 °C

560 - 620 MPa

Show Material materials with Yield strength of 560 - 620 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

Specific heat capacity

20.0 °C

430 J/(kg·K)

Show Material materials with Specific heat capacity of 430 J/(kg·K)

Thermal conductivity

20.0 °C

40 W/(m·K)

Show Material materials with Thermal conductivity of 40 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

2.6E-7 Ω·m

Show Material materials with Electrical resistivity of 2.6E-7 Ω·m

Chemical properties

PropertyValue

Boron

5E-3 %

Show Material materials with Boron of 5E-3 %

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Chromium

1.5 %

Show Material materials with Chromium of 1.5 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Manganese

1.7 %

Show Material materials with Manganese of 1.7 %

Molybdenum

0.7 %

Show Material materials with Molybdenum of 0.7 %

Nickel

2 %

Show Material materials with Nickel of 2 %

Niobium

0.06 %

Show Material materials with Niobium of 0.06 %

Nitrogen

0.02 %

Show Material materials with Nitrogen of 0.02 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

Vanadium

0.12 %

Show Material materials with Vanadium of 0.12 %

Zirconium

0.15 %

Show Material materials with Zirconium of 0.15 %