EN 10137-3 Grade S550AL quenched and tempered (+QT)

View suppliers (1)
Want to keep this datasheet? Save it now in your required format

Description

S550AL is a precipitation hardening and weldable fine grained steel. yield point: >550 N/mm² application: welded steel constructions of various types, e.g. bridges and load-carrying constructions as well as transport vehicles, lifting and earthmoving machines. application limits: at -40°C is warranted a notch impact energy of 40 J (longitudinal test specimen) cold formability: for nominal size < 16 mm bending radius in transversal direction 3xs in longitudinal direction 4xs (s= nominal thickness) hot forming property: allowed only for stress relieve annealing temperature (max. 580°C) suitability for welding: Steel is weldable according to the common welding methods (EURONORM-INFORMATION Nr. 2 has to be considered)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

16 %

Show Material materials with Elongation of 16 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

650 - 820 MPa

Show Material materials with Tensile strength of 650 - 820 MPa

Yield strength

20.0 °C

530 - 550 MPa

Show Material materials with Yield strength of 530 - 550 MPa

Chemical properties

PropertyValue

Carbon

0.03 - 0.12 %

Show Material materials with Carbon of 0.03 - 0.12 %

Manganese

0.3 - 1.8 %

Show Material materials with Manganese of 0.3 - 1.8 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %